Sandvik 6EF Extra-fine Grain Cemented Carbide for Rotary Tools

 

Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal

Material Notes:
SANDVIK extra-fine grain cemented carbide grades have been developed to meet the exacting demands placed on solid carbide tooling by modern technology.

The range of SANDVIK extra-fine grain cemented carbide grades have a tungsten carbide grain size of 0.6 µm. This grain size is precisely controlled to produce a tool material with an excellent combination of strength and toughness. In addition, a special additive maximises corrosion resistance without loss of toughness.

SANDVIK grade 6EF has been developed as a result of an extensive research programme aimed at optimising solid carbide tool performance in metal cutting applications.

6EF incorporates 6% cobalt (Co) and 94% tungsten carbide (WC). 6EF is recommended for solid carbide rotary tool applications in the ISO K05/K10 range. It has special advantages where high toughness, sharp edge profiles and exceptional wear resistance is required.

Information provided by Sandvik

Available Properties
  • Density
  • Hardness, Rockwell A
  • Hardness, Vickers
  • Rupture Strength
  • Compressive Strength
  • Corrosion Resistance, 1-10
  • Wear Resistance, 0-10
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。