Subscribe to FREE Trade Publications!

Sandvik 1802 Precision Wire

 

Subcategory: Stainless Steel; Alloy Steel; Metal; Ferritic

Close Analogs: EN 1.4523

Material Notes:

  • Very good machinability High productivity and low production cost. Substantial benefits in the form of increased production speed and reduced tool wear compared with steels of type AISI 316L with improved machinability.
  • Superior corrosion resistance Replacement of high alloyed steels.
  • Simplified stock keeping Suitable for a wide range of applications.
  • Sandvik 1802 is a ferritic stainless free-cutting steel, alloyed with titanium and sulphur. It is superior in all applications involving a sufficiently high cutting speed, preferably 200 - 300 m/min. The excellent machinability results in superior surface finish.Also in operations where low cutting forces and/or excellent chip flow, e.g. grooving, internal turning or drilling are an advantage, Sandvik 1802 can offer improved production economy.

    Service temperature -60 to 300°C. Scaling temperature in air 850°C.

    Information provided by Sandvik

    Available Properties
    • Density
    • Tensile Strength, Ultimate
    • Tensile Strength, Ultimate at Elevated Temperature
    • Tensile Strength, Yield
    • Tensile Strength, Yield at Elevated Temperature
    • Elongation at Break
    • Elongation at Break at Elevated Temperature
    • Modulus of Elasticity
    • Electrical Resistivity
    • Magnetic Permeability
    • Magnetic Coercive Force, Hc
    • Magnetic Saturation Flux Density, Bmax
    • Magnetic Remanence, Br
    • CTE, linear 100°C
    • CTE, linear 250°C
    • CTE, linear 500°C
    • Specific Heat Capacity
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。