MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Sandvik Nanoflex Strip Steel

 

Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal; Austenitic

Material Notes:
Sandvik Nanoflex® is a precipitation hardenable, austenitic stainless steel specifically designed for applications requiring high strength and good ductility. The mechanical strength can be remarkably increased by heat treatment (ageing) of the final product, first taking advantage of a soft as-delivered condition favourable for forming. Normally the material is delivered in cold rolled condition, but there is also a possibility to use the grade in annealed condition and still reach a comparably high strength solely by heat treatment.

Sandvik Nanoflex® is characterized by:

  • very high tensile strength can be reached, still with comparably good ductility
  • very high ageing effect
  • hardenable by heat treatment from annealed condition
  • no softening after exposure to temperatures up to 450°C
  • good weldability
  • The grade is also known under the in-house designation Sandvik 1RK91.

    Information provided by Sandvik

    Available Properties
    • Density
    • Tensile Strength, Ultimate
    • Tensile Strength, Ultimate at Elevated Temperature
    • Modulus of Elasticity
    • CTE, linear 100°C
    • CTE, linear 500°C
    • Specific Heat Capacity
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。