Nucalloy® 488V High-Silicon, Nickel-Base Hardfacing Alloy

 

Subcategory: Superalloy; Nonferrous Metal; Nickel Base

Key Words: Deloro Stellite Inc.

Material Notes:
Nickel content above calculated as balance.

Applications include diesel engine valves, and injection mold screws.

Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness and toughness, similar to the cobalt base alloys . Because of the unique microstructure features, they are less crack sensitive than the conventional nickel-base hardfacing alloys, such as, NiCr-A and NiCr-B, during welding.

The Nucalloy alloys have a matrix consisting of, essentially, nickel solid solution, a binary eutectic and ternary eutectic. The binary eutectic is composed of nickel solid solution and nickel silicide (Ni3Si); whereas the ternary eutectic consists of nickel solid solution, nickel boride (Ni3B) and nickel silicide (Ni3Si). There are also carbide and boride particles dispersed in the matrix. The microstructures of these alloys differ from those of the conventional self-fluxing nickel alloys in that the brittle binary eutectic of nickel solid solution and nickel boride does not form because of the intentionally controlled high silicon to boron ratios.

The high silicon and low boron in these alloys results in high fractions of nickel silicide, which is resistant to certain corrosive media due to the tendency to form a high-silicon film on the surface.

Information provided by Deloro Stellite Inc.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Charpy Impact Unnotched
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。