Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S)

 

Subcategory: Tool Steel; Alloy Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addition, the alloy sulfides improve grindability in the hardened condition and make the steel machinable by conventional chip-cutting techniques if the hardness is kept below about 46 HRC. A steel having the same chemical composition, but which is prehardened to 42 to 46 HRC is sold as Viscount 44. Both Viscount 20 and Viscount 44 are excellent selections for numerous hot work and cold work tooling applications where machinability is of primary importance.

Information Provided by Timken Latrobe Steel.

Available Properties
  • Specific Gravity
  • Density
  • Critical Temperature
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Machinability
  • CTE, linear 20°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。