Latrobe LSS™ D7 Tool Steel (ASTM D7)

 

Subcategory: Tool Steel; Air-Hardening Steel; High Carbon Steel; Alloy Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide particles in the steel. These carbides exhibit a hardness that is equivalent to approximately 80 to 85 Rockwell C. TLS D7 tool steel resists wear from sliding contact with other steels as well as from contact with dry and wet slurries of hard abrasive particles such as sand, shot blast media, and ceramics. Typical applications include brick mold liners, briquetting dies, shot blasting equipment liners, tools for ceramic extrusion and molding, powder compaction tooling, deep drawing dies, flattening rolls, and machine tool ways.

Information Provided by Timken Latrobe Steel.

Available Properties
  • Hardness, Rockwell C
  • Izod Impact Unnotched
  • Machinability
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。