Eastman SP 2268T EMAC® Ethylene-Methyl Acrylate Copolymer

 

Subcategory: Ethylene Methyl Acrylate; Thermoplastic

Key Words: Eastman EMAC

Material Notes:
24% Methyl Acrylate Content.

Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing Up to 600°F, Non-Corrosive at Extrusion Temperatures

Applications:Compounding: Impact Modification, Compatibilizer, Masterbatch Base Resin; Coatings & Laminations: Higher Neck-In but Similar Drawdown vs. LDPE Extrusion Coating Grades, Excellent Heat Seal Response at Low Seal Temperatures, Adheres Very Well to Non-Porous Substrates such as OPP, PVDC Coated Substrates, and Polyester, Adheres Well to Porous Substrates such as Paper and Paperboard

Data provided by Chevron Chemical. Chevron sold its EMAC® and EBAC® product lines to Eastman Chemical in 1999.

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Melt Flow
  • Hardness, Shore A
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Melting Point
  • Vicat Softening Point
  • Brittleness Temperature
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。