Evoprene® Super G 949 Thermoplastic Elastomer, Unreinforced

 

Subcategory: Elastomer, TPE; Thermoplastic

Key Words: TPE; LAPORTE AlphaGary

Material Notes:

Characteristics: Excellent Low Temperature Properties, Excellent Bond Strength with Polypropylene

Applications: Window & Door Seals, Gaskets, Grips & Handles, Automotive Trim, Electrical Insulators

Processing: Injection Molding (Melt: 390-430°F, Mold: 105-140°F); Extrusion (Melt: 375-430°F)

Ozone resistance (35°C; 100 pphm/200hrs/20% strain: No Cracks
UV Resistance; 1500 hrs @ 40°C QUV (black): Excellent
Air Aged 14 Days @ 125°C: 110% retained T/S. 110% retained E/B. Hardness change: +2.
Air Aged 7 Days @ 150°C: 110% retained T/S. 111% retained E/B. Hardness change: +2.

Evoprene® is a registered trademark of LAPORTE AlphaGary, LTD.

Available Properties
  • Density
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Tear Strength
  • Abrasion
  • Compression Set
  • Compression Set, Elevated Temperature
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Processing Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。