Honeywell Capran® NyLid™ WMB 250, Nylon Lidding Film

 

Subcategory: Ethylene Vinyl Alcohol; Nylon; Thermoplastic; Polymer

Material Notes:
Description: Capran® NyLid™ WMB 250 is a 2.5 mil, white medium barrier nylon co-extruded film with an EVOH core.

Applications: Capran® NyLid™ WMB 250 is suitable for die cutting, readily accepts printing, accepts heal seal coatings and lacquers, offers excellent puncture resistance, is safe for microwave use, and resists tear propagation. It is ideally suited for lamination, and is FDA compliant for indirect food contact.

Information provided by Honeywell.

Available Properties
  • Density
  • Water Vapor Transmission
  • Oxygen Transmission Rate
  • Thickness
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Tear Strength Test
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Shrinkage, MD
  • Shrinkage, TD
  • Gloss
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。