Honeywell ETFE EX30, Mono-Axially Oriented, ETFE Film

 

Subcategory: Nylon; Thermoplastic; ETFE/ECTFE; Polymer

Material Notes:
Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistance, exceptional clarity and enhanced mechanical properties. It is widely used as a protective film for long term outdoor applications like retro-reflective signage and photovoltaic cells.

Information provided by Honeywell.

Available Properties
  • Specific Gravity
  • Density
  • Moisture Absorption at Equilibrium
  • Water Vapor Transmission
  • Thickness
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Film Elongation at Yield, MD
  • Film Elongation at Yield, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Melting Point
  • Oxygen Index
  • Shrinkage, MD
  • Shrinkage, TD
  • Refractive Index
  • Haze
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。