COIM LARIPUR® LPR6325 Special Adipate Ester Polyurethane

 

Subcategory: Polyester, TP; Polyurethane, TP; Thermoplastic

Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:

  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 25 Special Adipate Ester: These products are based on saturated polyesters. Products are based on saturated polyester. The features are similar to those of Series 20 but, by comparison, they are characterized by a higher resistance to hydrolysis and improved flexibility at low temperatures.
Information provided by P.A.T. Products, Inc.

Available Properties
  • Specific Gravity
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • 50% Modulus
  • 100% Modulus
  • 300% Modulus
  • Flexural Modulus
  • Izod Impact, Notched, Low Temp (ISO)
  • Tear Strength
  • Abrasion
  • Torsional Stiffness
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。