DuPont Teflon® PTFE Grade K-20 Aqueous Dispersion

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts

Material Notes:
Teflon® PTFE K-20 is a negatively charged, hydrophobic colloid containing approximately 33% (by total weight) of 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles suspended in water. A milky white liquid, Teflon® PTFE K-20 also contains approximately 3.5% (by weight of PTFE) of a nonionic wetting agent and stabilizer. Viscosity at room temperature is approximately 15 cPs. Nominal pH is 10.

Teflon® PTFE K-20 is used in applications where a minimum amount of surfactant is desired. The most common use for Teflon® PTFE K-20 is to reduce dust levels in host systems. When sheared, micro fibrils of PTFE are formed that interconnect the 0.2 mm particles. The presence of these micro fibrils reduces dust levels in many host systems.

When properly processed, the PTFE resin in Teflon® PTFE K-20 exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

Typical products that have been successfully de-dusted include carbon powder, catalysts, fine chemicals, cement, and clays such as those in cat litter.

Available Properties
  • Specific Gravity
  • Base Resin Density
  • Solids Content
  • Particle Size
  • pH
  • Viscosity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。