DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating

 

Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer

Key Words: DuPont Packaging Polymers

Material Notes:
6.5 wt% Methacrylic Acid.

Nucrel® 0609HSA is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins. This resin may also be used in conventional blown and cast film extrusion and coextrusion equipment.

Features & Benefits: Excellent adhesion to unprimed foil, paper and metallized film provides better substrate protection, improved structure reliability, and barrier integrity. This product provides very good but lower adhesion to polyethylene than acid copolymers with 4% or less methacrylic acid content (e.g., Nucrel® 0407 and Nucrel® 0411HS). High speed operation on packaging machinery is enhanced by low seal initiation temperature compared to LDPE Excellent hot tack, sealability through contamination, and heat seal strength provides strong, reliable heat seals Contains anti-oxidant.

Typical Applications: Foil-containing pouches and sachets; Aseptic and hot-fill liquid cartons; Lidding and snack structures; Other foil, metallized film, or paper coatings as a heat seal or tie layer.

Information provided by DuPont Packaging Polymers.

Available Properties
  • Melt Flow
  • Melting Point
  • Vicat Softening Point
  • Processing Temperature
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。