Polimeri Europa Edistir N 2982 Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Material Notes:
General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC and HCFC. Low viscosity process-aid and modifyer for compounding.

Designation: Thermoplastics ISO 1622-PS,E,105-20

Applications: XPS insulation panels with improved environmental compatibility. Carrier for masterbatch. Modifyer for thermoplastic elastomers and rubbers (shoe soles, cable extrusion-coating).

N 2982 is certified UL94 HB "all colors" at 1.5 mm (UL file E83071).

This grade in its natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (including the EEC Directive 90/128 and subsequent amendments).

Information provided by Polimeri Europa

Available Properties
  • Density
  • Bulk Density
  • Water Absorption
  • Melt Flow
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Flexural Strength
  • CTE, linear 20°C
  • Thermal Conductivity
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。