Equistar Ultrathene® UE635000 Ethylene Vinyl Acetate Copolymer, Extrusion Coating Grade

 

Subcategory: Ethylene Vinyl Acetate; Equistar Ethylene Vinyl Acetate

Material Notes:
ULTRATHENE UE635000 is an ethylene vinyl acetate copolymer recommended for extrusion coatings on cellophane, polypropylene and polyester. UE635000 is also used in special coextruded substrate coating applications, yielding improved heat stability for snack food packaging.

Regulatory Status: UE635000 is sanctioned by Food and Drug Administration regulation Federal 21 CFR 177.1350 and 21 CFR 175.105. These regulations (respectively) allow for the use of this material as articles or components of articles which are "...intended for use in producing, manufacturing, packing, processing, preparing, treating, packaging, transporting or holding food..." and as an adhesive which "...may be safely used as components of articles intended for use in packaging, transporting or holding food." Specific limitations or conditions of use may apply. Please contact your Equistar sales representative for more information regarding the suitability of specific products for specific applications.

Processing Techniques: The maximum recommended melt temperature for UE635000 is 450°F. Specific recommendations for processing UE635000 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.

Available Properties
  • Density
  • Vinyl Acetate Content
  • Melt Flow
  • Vicat Softening Point
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。