Total 3365 Polypropylene, Extrusion Grade

 

Subcategory: Polypropylene; Thermoplastic

Close Analogs:

Total Petrochemicals now includes former Fina and Atofina plastics product lines.

Material Notes:
Homopolymer extrusion grade for water quench slit film

Low Water Carryover - Fina 3365 exhibits excellent low water carryover which allows extrusion at maximum line speeds.

High Purity - Low catalyst residues in FINA 3365 allow extended processing runs without screen pack pluggage.

FDA - Fina 3365 complies with all applicable FDA regulations for food contact applications.

Recommended Applications FINA 3365 is recommended for water quench slit films and monofilaments for carpet backing, rope, and cordage products.

Processing - FINA 3365 processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C).

Data provided by the manufacturer, Total Petrochemicals.

Available Properties
  • Density
  • Melt Flow
  • Tensile Strength, Ultimate
  • Tenacity
  • Modulus of Elasticity
  • Flexural Modulus
  • Melting Point
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。