Finaprene® 411 X Styrene-Butadiene TPE Copolymer Compound

 

Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic

Close Analogs:

Total Petrochemicals now includes former Fina and Atofina plastics product lines.

Material Notes:
Styrene-Butadiene Copolymer

Description: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides excellent mechanical and elastic properties to compound.

Applications: Thanks to its high molecular weight Finaprene® 411x is designed for the compounding industry. This crumb shape, along with the high molecular weight confer a quick and important oil absorption capacity to the polymer and lead tot eh production of economical compounds while keeping good mechanical properties.

Content of the compound for which the listed properties apply:
F484: 81
F435: 36
F411X: 10
Oil: 40
GPPS: 20
HIPS: 20
CaCO3: 15

Additional Notes:
DIN Abrasion: 195 mm³
Rossflex 100%: 40000 cycles
Rossflex 300%: 75000 cycles
Rossflex 500%: 117000 cycles

Data provided by Total Petrochemicals.

Available Properties
  • Viscosity Measure
  • Melt Flow
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flex Crack Resistance
  • Abrasion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。