Finaprene® 435 Styrene-Butadiene TPE Copolymer Compound

 

Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic

Close Analogs:

Total Petrochemicals now includes former Fina and Atofina plastics product lines.

Material Notes:
Styrene-Butadiene Copolymer

Description: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excellent mechanical properties and abrasion resistance to the compound along with a good fluidity.

Applications: Thanks to its very high crumb porosity Finaprene® 435 is designed rot he compounding industry. This crumb shape, along with the medium molecular weight confer a quick and important oil absorption capacity to the polymer and lead to the production of high quality compounds with good MFI.

Content of the compound for which the listed properties apply:
F484: 105
F435: 30
Oil: 40
GPPS: 20
HIPS: 20
CaCO3: 15

Additional Notes:
DIN Abrasion: 190 mm³

Data provided by Total Petrochemicals.

Available Properties
  • Viscosity Measure
  • Melt Flow
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 300% Modulus
  • Tear Strength
  • Abrasion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。