Greene Tweed FPD Blue™ 707 Fluoroelastomer

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Material Notes:
Specifically developed for flat panel display CVD and dry plasma etch equipment where seal reliability and minimal contamination are essential, FPD Blue™ 707 fluoroelastomer provides excellent chemical compatibility and withstands a variety of aggressive chemicals. Available in an infinite range of geometries and cross sections, this material offers the diversity required for a variety of dynamic or static dry processing applications. FPD Blue 707 remains stable at service temperatures up to 220°C (428°F) and is ideally suited for large lid seals and bonded slit valve door seals.

Applications:

  • Endpoint Windows
  • Valve seals
  • KF fitting seals
  • Window seals
  • Lid seals
  • Gas inlet seals
  • Slit valve seals
  • Chamber seals

Information provided by Green Tweed

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • Tensile Modulus
  • Compression Set
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。