Ipiranga Petroquímica LB 0120 BS LLDP

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer

Material Notes:
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and bags.

IPQ employs Spherilene technology from Montell/Italy in the production of LLDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where linear low density polyethylene globe-shaped grains are obtained. These grains are sent to the extrusion site, where stabilizers are added to them. The grains are turned into pellets by an extruding press. Next, they are sent to storage silos, and then to the packaging site. This technology uses state-of-the-art techniques to control the entire production process, thus ensuring the quality of the products that are marketed.

Applications:

  • blend with HDPE and LDPE for several applications

Available Properties
  • Density
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Film Elongation at Yield, MD
  • Film Elongation at Yield, TD
  • Coefficient of Friction
  • Dart Drop Test
  • Haze
  • Gloss
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。