KiON URETHANE HYBRID CLEAR COAT Pack B Heat-Curable Polysilazane-Based Hybrid Spray Coat

 

Subcategory: Thermoset; Polymer

Material Notes:
General Description

KiON Urethane Hybrid Clear Coat is a ready-to-use clear coat containing both polysilazane and polyurethane components that can be thermally-cured to provide an oxidation and corrosion-resistant clear or pigmented finish. KiON Urethane Hybrid Clear Coat is furnished as a 2-Pack system that can be applied by spray, dip, and brush coating techniques. It cures upon heating to temperatures of between 293 °F and 311 °F for 1 hour. KiON Urethane Hybrid Clear Coat provides a clear, protective coating for both ferrous and non-ferrous metals and alloys, ceramics, glass, etc. In addition, KiON Urethane Hybrid Clear Coat has excellent “weatherability”, UV resistance, hardness and abrasion resistance.

Applications

Clear, protective coatings for both ferrous and non-ferrous metals and alloys, clear automotive finishes, thermally durable coatings, and industrial, infrastructure and marine coatings.

Information provided by KiON Corporation

Available Properties
  • Density
  • Volatile Organic Compounds (VOC) Content
  • Viscosity
  • Flash Point
  • Gloss
  • %Resin
  • Appearance
  • Pencil Hardness ASTM D 3363
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。