Kydex® 101 Acrylic/PVC Thermoplastic Sheet

 

Subcategory: Vinyl; Acrylic; Thermoplastic

Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate

Material Notes:
Thermoplastic sheet for signage

Applications: Sign applications, radomes, other applications where a weatherable color over a white substrate is desirable

Features: Kydex 101 is more rigid than most other thermoplastics resulting in parts that will deform less when loaded. Offers unsurpassed resistance to breakage. The cap offers excellent weatherability for use in outdoor applications. Since the substrate is white, it eliminates the need for painting which is required with other thermoplastics and with metal.

Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.

Data provided by the Kleerdex Company.

Available Properties
  • Density
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。