LG Chemical KEYFLEX BT-1055D Thermoplastic Ester for Injection Molding, 55D Hardness

 

Subcategory: Polyester, TP; Elastomer, TPE; Thermoplastic

Material Notes:
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber and the strength of engineering plastics. In additions, they offer very good thermal stability, chemical resistance and weather resistance. KEYFLEX resins can be widely accepted as the replacement of thermoset rubbers.

Characterization:

  • High impact strength
  • Low specific gravity
  • Excellent resistance to chemicals and weathering
  • Good electrical properties
  • Various hardness grades (soft, semi-soft, and hard)
  • Colorability
  • Recyclability

Applications:

    Automotive: Bumper, timer ELR parts, safety belt hook, packing parts, actuator, fuel tank, remote control button

    Cable: Cable insulation, high pressure hose, wire clamp, telephone wire, computer cord, nut seal, seal parts

    Electrical and Electronic: Connector cover, connector, rubber switch, spring, timing belt

    Others: Film and sheet, packingless cap, hose, flexible coupling packing, conveyor belt, sealing parts.

Information Provided by LG Chem

Available Properties
  • Specific Gravity
  • Water Absorption
  • Linear Mold Shrinkage
  • Melt Index of Compound
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Tear Strength
  • Izod Impact, Notched @ -40°C
  • Izod Impact, Notched
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Injection Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。