LG Chemical TR-300 Transparent ABS, Flame Retardant, Natural and Colored Pellets

 

Subcategory: ABS Polymer; Thermoplastic

Material Notes:
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electronic parts, OA machines, toys and others that require transparency and high impact strength. An Izod impact strength or falling dart impact strength of LG transparent ABS is relatively similar to that of general ABS, it is not easily cracked like SAN or PMMA resin in the condition of low impact energy.

Information Provided by LG Chem

Available Properties
  • Specific Gravity
  • Linear Mold Shrinkage
  • Melt Index of Compound
  • Hardness, Rockwell R
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Haze
  • Transmission, Visible
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Adapter Temperature
  • Die Temperature
  • Melt Temperature
  • Mold Temperature
  • Roll Temperature
  • Injection Pressure
  • Back Pressure
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。