Cookson Group STAYCHIP® 3082 High Reliability Flip Chip Underfill, Low CTE

 

Subcategory: Adhesive; Thermoset

Material Notes:
STAYCHIP™ 3082 is a highly filled, high reliability capillary underfill designed for high performance applications. This material provides superior adhesion to common solder-mask and die passivations, even after exposure to elevated heat, pressure, and humidity for superior JEDEC performance. This fast flow underfill was formulated for penetration of gaps below 1 mil. When fully cured, the material displays excellent reliability in thermal cycling performance. It is easily dispensed and exhibits low moisture absorption for improved JEDEC performance.

Features:

  • Excellent reliability in thermal cycling
  • Excellent Reliability in JEDEC testing
  • Low CTE
  • High Tg
  • Exceptional adhesion (even after exposure to high humidity, pressure, and temperature)
  • Fast, efficient flow properties
  • Small particle size filler for use on fine pitch array packages
  • High filler loading while maintaining fast flow properties

Information provided by Cookson Electronics

Available Properties
  • Specific Gravity
  • Filler Content
  • Moisture Absorption at Equilibrium
  • Viscosity
  • Storage Temperature
  • Hardness, Shore D
  • Adhesive Bond Strength
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • Glass Temperature
  • Flash Point
  • Pot Life
  • Shelf Life
  • Appearance
  • Chemical Type
  • Etractable Ionic Contant, Chloride (Cl)
  • Etractable Ionic Contant, Potassium (K)
  • Etractable Ionic Contant, Sodium (Na)
  • Particle Size
  • Storage Modulus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。