UBE UBEPOL-VCR412 New Type Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)

 

Subcategory: Elastomer, TS; Thermoset

Material Notes:
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high melting point and crystallinity, and high cis-1,4-polybutadiene rubber matrix. UBEPOL-VCR is improved on the processability and a lot of physical properties of the conventional polybutadiene rubber (BR).

Information provided by UBE.

Available Properties
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • 100% Modulus
  • 200% Modulus
  • 300% Modulus
  • Rebound
  • Tear Strength
  • Abrasion
  • Compression Set
  • Cut Generation De Mattia Flexing Machine
  • Cut Growth (2mm-->15mm)  De Mattia Flexing Machine
  • Goodrich Flex,  0.175" Stroke, 55lb, 100°C, P.S.
  • Wet Skid Resistance on Safety-Walk
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。