UBE UPISEL-N BE1210 Copper Clad Laminate

 

Subcategory: Metal

Material Notes:
Description: UPISEL-N BE1210 is non-adhesive type flexible Copper Clad Laminate (Polyimide = 25µm, Cu = 18µm) based on "UPILEX-VT." UPISEL-N has excellent dimensional stability and heat resistance. "UPILEX-VT" performs high bonding ability without any use of adhesives by simple heat lamination. "UPILEX-VT" is an aromatic polyimide same as "UPILEX-S" which has high market share as the base film for TAB (Tape Automated Bonding).

Applications:

  • FPC
  • TCP
  • MCM-L
  • COF
  • Rigid flex
  • Multi-layer boards
  • Metal based boards
  • High frequency boards
  • Heat-resistant boards
  • IC cards
  • Boards for automobile
  • Electromagnetic wave shield material
  • HDD suspension

Characteristics:

  • Without the use of adhesives, UPISEL-N maintains high physical properties and high reliability at high temperatures
  • It performs excellent peeling strength, heat soldering resistance, chemical resistance and dimensional stability
  • The film layer of the UPISEL-N can be heat bonded with ceramics, metals and silicon chip
  • Without the use of adhesives, UPISEL-N is tender for the environment

Information provided by UBE.

Available Properties
  • Water Absorption
  • Elongation at Break
  • Tensile Modulus
  • Peel Strength
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Flammability, UL94
  • Shrinkage
  • Flexural Endurance (MD)
  • Flexural Endurance (TD)
  • Folding Endurance RO.4 (MD)
  • Folding Endurance RO.4 (TD)
  • Hot Solder Resistance: 300°C 1 min.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。