Conoco Syncon® Synthetic EP Gear Oil 680, AGMA No. 8EP

 

Subcategory: Fluid; Lubricant

Material Notes:
Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is suited for extruder reducers, agitator drives, centrifuge gear boxes and industrial gear drives of spur, helical, herringbone and bevel gear design that require severe-duty, extreme-pressure lubricants. It is also suited for ball, roller and needle antifriction bearings. Syncon Synthetic EP Gear Oil is available in five ISO viscosity grades: 150, 220, 320, 460 and 680.

Information provided by ConocoPhillips.

Available Properties
  • Density
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Load Wear Index
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Timken Test
  • Pour Point
  • Flash Point
  • ASTM Rust A&B
  • Copper Corrosion
  • Demulsibility: Emulsion
  • Demulsibility: Freewater
  • Foam: Sequence I
  • Foam: Sequence II
  • Foam: Sequence III
  • FZG Gear Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。