PolyOne Geon® 1410-xx61FRD Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized Insulation per UL QMTT2
- TW
- THW
- THHN
- THWN
- UL 105°C
- Flame Retardant
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.33 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 90 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 2900 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 280 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Electrical Properties |
|
Volume Resistivity | 1e+015 ohm-cm | ASTM D257 |
Thermal Properties |
|
Brittleness Temperature | -31 °F | ASTM D746 |
Oxygen Index | 28 % | 0.075 in; ASTM D2863 |
Processing Properties |
|
Melt Temperature | 345 - 355 °F | Extrusion |
Descriptive Properties | |
Oven Aged - Retention of Elongation (ROE) | 70 % | 277°F (136°C), 168 hrs (7 days), 0.075 in; UL Standard |
Oven Aged - Retention of Tensile Strength (ROT) | 95 % | 277°F (136°C), 168 hrs (7 days), 0.075 in; UL Standard |
Product Form | Pellets/Cubes | |
|