PolyOne Geon® 171 Polyvinyl Chloride Homopolymer (PVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Good dispersability in both organosol and plastisol formulations
- Low residual emulsifier level 1.5-1.6% provides good clarity, moisture blush resistance
- Low taste and odor
- Fine grind and stable viscosity characteristics for thin film applications
- Low Brookfield and Severs viscosities for easy processing
- Ultra High Molecular Weight Resin Providing Excellent Fused Film Properties
Applications: - Recommended where a balance of fusion and rheological properties are required
- Thin film organosols and plastisols
- Resilient flooring wear layer
- Strand Coating
- Organosol coatings
Dispersion Polymerization ProcessDisclaimer: Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: The values set forth represent "typical" values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Manufacturing Location: This resin is produced at PolyOne Corporation's Henry, IL facility, which is ISO 9002 certified. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Information provided by PolyOne Corporation.
We're sorry, but our sources do not report any other information for this material. We are limited by the information available from our sources, which often are not as complete as we would like. Sometimes you will see this message during a MatWeb internal update, especially around 07:00 GMT Sundays.
|