MatWeb, The Online Materials Database

SPHERE ONE EXTENDOSPHERES™ PM 6550 Hollow Spheres


Subcategory: Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes:
PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide substantial volume filling in formulations. PM 6550 has excellent flexibility, and the walls of the hollow sphere can survive a variety of stress environments. PM 6550 offers good resistance to solvents. The oleophilic surface permits easy dispersion in organic fluids and resins, but also provides good wet-out in latex systems.

Applications: PM 6550 can be used to cover the whole range of applications where Sphere One hollow spheres would be incorporated. Plastic hollow spheres have found utility in such wide ranging applications as emulsion explosives, autobody putties, sealants and epoxy syntactic foams.

Information provided by Sphere One Inc.

Physical PropertiesMetricEnglishComments
Density0.03 g/cc0.00108 lb/in³ 
Bulk Density0.05 g/cc0.00181 lb/in³ 
Particle Size10 - 200 µm10 - 200 µm 
Particle Size100 µm100 µm Average Mean

Thermal Properties
Maximum Service Temperature, Air140 °C284 °F Deformation temp

Descriptive Properties
ColorOff White 
Physical FormFree-Flowing Powder 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.