MatWeb, The Online Materials Database

Bismuth Selenide, Bi2Se3


Subcategory: Ceramic; Semiconductor; Sulfide/Chalcogenide

Key Words: Chalcogenide; Semiconductor; Selenium

Physical PropertiesOriginal ValueComments
Density7.51 g/cc 
a Lattice Constant4.14 Å 
c Lattice Constant28.7 Å 
Molecular Weight654.84 g/mol 

Mechanical Properties
Knoop Microhardness167 N/mm²

Electrical Properties
Band Gap0.35 eV 
Electron Mobility, cm²/V-s600 

Thermal Properties
Thermal Conductivity2.4 W/m-K 
Melting Point706 °C 

Descriptive Properties
CAS Number12068-69-8 
ColorBlack 
Crystal StructureHexagonal-Rhombohedral Tetradymite Structure - R(-3)M

References are available for this material.

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.