MatWeb, The Online Materials Database

Bismuth Telluride, Bi2Te3 (Tellurobismuthite)


Subcategory: Ceramic; Semiconductor; Sulfide/Chalcogenide

Key Words: Chalcogenide; Semiconductor; Tellurium

Physical PropertiesMetricEnglishComments
Density7.73 g/cc0.279 lb/in³ 
a Lattice Constant4.38 Å4.38 Å 
c Lattice Constant30.45 Å30.45 Å 
Formula Units/Cell (Z)33 
Molecular Weight800.76 g/mol800.76 g/mol 

Mechanical Properties
Knoop Microhardness155155 N/mm²
Hardness, Mohs1.81.8 

Electrical Properties
Band Gap0.21 eV0.21 eV 
Electron Mobility, cm²/V-s11401140 
Hole Mobility, cm²/V-s680680 

Thermal Properties
Specific Heat Capacity0.016 J/g-°C0.00382 BTU/lb-°F 
Thermal Conductivity3 W/m-K20.8 BTU-in/hr-ft²-°F 
Melting Point585 °C1090 °F 

Descriptive Properties
CAS Number1304-82-1 
ColorGray 
Crystal StructureHexagonal-Rhombohedral Tetradymite Structure - R(-3)M
SolubilityInsoluble in H2O; Soluble in EtOH 

References are available for this material.

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.