MatWeb, The Online Materials Database
Aluminum Alloys, General
Subcategory: Aluminum Alloy; Metal; Nonferrous Metal
Key Words: Aluminium Alloys, General; Al Alloys
| Component | Wt. % |  | | | Al | 87 - 100 | |
|
Material Notes: These properties are typical of commercial aluminum alloys. Some properties, such as strength and hardness, vary too much for a reasonable generalization. See entries for individual alloys for more specific information. Aluminum 1199 is the highest purity (99.99% Al min.) in the database.
| Physical Properties | Metric | English | Comments |
|
| Density | 2.7 g/cc | 0.0975 lb/in³ | |
Mechanical Properties |
|
| Modulus of Elasticity | 70 GPa | 10200 ksi | |
| Poisson's Ratio | 0.33 | 0.33 | |
| Shear Modulus | 26 GPa | 3770 ksi | |
Electrical Properties |
|
| Electrical Resistivity | 5e-006 ohm-cm | 5e-006 ohm-cm | |
Thermal Properties |
|
| Heat of Fusion | 390 J/g | 168 BTU/lb | |
| CTE, linear 20°C | 24 µm/m-°C | 13.3 µin/in-°F | from 0-100°C (32-212°F) |
| CTE, linear 250°C | 25 µm/m-°C | 13.9 µin/in-°F | |
| Specific Heat Capacity | 0.88 J/g-°C | 0.21 BTU/lb-°F | |
| Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
| Melting Point | 620 - 650 °C | 1150 - 1200 °F | |
| Solidus | 620 °C | 1150 °F | |
| Liquidus | 650 °C | 1200 °F | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |