MatWeb, The Online Materials DatabaseAdvanced Elastomer Systems Santoprene® 121-50 M100 Thermoplastic RubberSubcategory: Elastomer, TPE; Polymer; Thermoplastic Material Notes: Key Features: Fast, easy injection molding, especially for complex part geometries; Good sealing performance; Excellent surface aspect; Excellent elastic recovery up to 100°C (212°F); Minimal part warpage; Can be injected at lower molding temperatures or at lower injection pressures Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Copyright 1996-2010 by Automation Creations, Inc. The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb. |