Advanced Elastomer Systems Santoprene® 123-40 Thermoplastic Rubber


Subcategory: Elastomer, TPE; Polymer; Thermoplastic

Material Notes:
A black thermoplastic UV grade elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques.

Key Features: Dielectric constant 2.3, dielectric strength at 3.17 mm (125 mil), 19.6 kV/mm (500 v/mil); Flame resistant HB material; Continuous temperature rating 1000 hrs. @ 135°C (275°F); Excellent flex fatigue resistance; Excellent ozone resistance; Excellent UV resistance

Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

Physical PropertiesMetricEnglishComments
Density0.95 g/cc0.0343 lb/in³ TPE-0105 (ASTM D792)

Mechanical Properties
Hardness, Shore D4040 5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate16.5 MPa2390 psi TPE-0153 (ASTM D 412)
Elongation at Break650 %650 % TPE-0153 (ASTM D 412)
100% Modulus0.0091 GPa1.32 ksi TPE-0153 (ASTM D 412)
Tear Strength65 kN/m371 pli 65 kN/m at 23°C. Value at 100°C is 36 kN/m. TPE-0056 (ASTM D 624)
Compression Set35 %35 % 23°C, 168 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature50 %50 % 100°C, 168 hrs.; TPE-0016 (ASTM D 412)
Tensile Set48 %48 % 23°C, 168 hrs.; TPE-0053 (ASTM D 412)

Electrical Properties
Dielectric Constant2.32.3 Frequency not specified
Dielectric Strength19.6 kV/mm498 kV/in at 3.17 mm (0.125 in)

Thermal Properties
Maximum Service Temperature, Air135 °C275 °F Continuous temperature Rating, 1000 hours
Brittleness TemperatureMax -57 °CMax -70.6 °F TPE-0089 (ASTM D 746)
Flammability, UL94HBHB 

Processing Properties
Processing Temperature177 - 232 °C351 - 450 °F 
Drying Temperature82 °C180 °F Desiccant drying for 3 hours recommended
Dry Time3 hour3 hour 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.