Advanced Elastomer Systems Santoprene® 181-64 Thermoplastic Rubber


Subcategory: Elastomer, TPE; Polymer; Thermoplastic

Close Analogs: This grade is no longer a commercial product

Material Notes:
A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Drug Master File has been established at US FDA National Center for drugs and biologics.

Key Features: MEM elution cytotoxicity to L-929 mouse fibroblast cells, 72 hr. exposure to rubber extract; NAmSA, MT023-100 test method; test unit, % cell lysis; typical value 0; USP physiochemical test for elastomer closures, heavy metals such as lead; NAmSA, CP020-004 test method; Test unit, ppm; typical value <1

Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

Physical PropertiesMetricEnglishComments
Density0.97 g/cc0.035 lb/in³ TPE-0105 (ASTM D792)

Mechanical Properties
Hardness, Shore A6464 5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate6.9 MPa1000 psi TPE-0153 (ASTM D 412)
Elongation at Break440 %440 % TPE-0153 (ASTM D 412)
100% Modulus0.0023 GPa0.334 ksi TPE-0153 (ASTM D 412)
Graves Tear Strength25 kN/m143 pli at 23°C. Value at 100°C is 10 kN/m. TPE-0056 (ASTM D 624)
Compression Set23 %23 % 23°C, 168 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature36 %36 % 100°C, 168 hrs.; TPE-0016 (ASTM D 412)
Tensile Set10 %10 % 23°C, 168 hrs.; TPE-0053 (ASTM D 412)

Thermal Properties
Brittleness TemperatureMax -60 °CMax -76 °F TPE-0089 (ASTM D 746)

Processing Properties
Processing Temperature177 - 232 °C351 - 450 °F 
Drying Temperature82 °C180 °F Desiccant drying for 3 hours recommended
Dry Time3 hour3 hour 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.