Advanced Elastomer Systems Santoprene® 201-68 W228 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Polymer; Thermoplastic
Material Notes: A colorable thermoplastic rubber with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. The product is designed to be processed using especially adapted physical foam extrusion lines. The product is polyolefin based and fully recyclable. Key Features: Water used as physical foaming agent; Density range 0.95 to 0.15 depending on foaming agent level; Excellent ozone resistance; Continuos temperature rating 1000 hrs @ 125°C Additional processing comments: Shear-dependent. For physical foaming a special modified thermoplastic extruder with adapted foaming agent dosing device is required. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
| Physical Properties | Original Value | Comments |
|
| Density | 0.97 g/cc | TPE-0105 (ASTM D792) |
| Apparent Bulk Density | 0.15 - 0.95 g/cc | Typical foam |
Mechanical Properties |
|
| Hardness, Shore A | 68 | 5 Second; TPE-0169 (ASTM D 2240) |
| Tensile Strength, Ultimate | 1.2 MPa | Typical foam value (ASTM D 412) |
| Tensile Strength, Ultimate | 6.9 MPa | TPE-0153 (ASTM D 412) |
| Elongation at Break | 400 % | TPE-0153 (ASTM D 412) |
| 100% Modulus | 0.0023 GPa | TPE-0153 (ASTM D 412) |
| Graves Tear Strength | 25 kN/m | 23°C. Value at 100°C is 10 kN/m. TPE-0056 (ASTM D 624) |
| Compression Set | 23 % | 23°C, 168 hrs.; TPE-0016 (ASTM D 412) |
| Compression Set, Elevated Temperature | 25 % | 70°C, 22 hrs.; TPE-0016 (ASTM D 412) typical foam value. |
| Compression Set, Elevated Temperature | 33 % | 100°C, 22 hrs.; TPE-0016 (ASTM D 412) typical foam value. |
| Compression Set, Elevated Temperature | 36 % | 100°C, 168 hrs.; TPE-0016 (ASTM D 412). |
| Tensile Set | 10 % | 23°C, 168 hrs.; TPE-0053 (ASTM D 412) |
Thermal Properties |
|
| Maximum Service Temperature, Air | 125 °C | Continuous temperature Rating, 1000 hours |
| Brittleness Temperature | Max -60 °C | TPE-0089 (ASTM D 746) |
Processing Properties |
|
| Drying Temperature | 70 - 90 °C | recommended. |
| Dry Time | 2 - 3 hour | recommended. |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |