BASF Ecoflex F BX 7011 Biodegradable, Aliphatic Aromatic Copolyester
Subcategory: Film; Polyester, TP; Polymer; Thermoplastic
Material Notes: Information provided by BASF Corporation.
Physical Properties | Metric | English | Comments |
|
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
Moisture Vapor Transmission | 140 cc-mm/m²-24hr-atm | 356 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness Unknown); DIN 53122 |
Oxygen Transmission Rate | 1600 cc/m²/day | 103 cc/100 in²/day | 23°C/0% RH; DIN 53380 |
Melt Flow | 3.45 g/10 min | 3.45 g/10 min | 190°C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
Elongation at Break | Min 50 % | Min 50 % | 50 mm/min; Nominal; ISO 527 |
Thermal Properties |
|
Melting Point | 112 °C | 234 °F | 10 K/min |
Optical Properties |
|
Transmission, Visible | 82 % | 82 % | ASTM D1003 |
Descriptive Properties | |
Color | Transparent | |
Commercial Status (March 2007) | North America and Europe | |
Impact Modified | No | |
Primary Processing Technique | Blown Film | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|