Physical PropertiesOriginal ValueComments
Density1.26 g/cc ISO 1183
Moisture Vapor Transmission140 cc-mm/m²-24hr-atm cc/m2/day (Thickness Unknown); DIN 53122
Oxygen Transmission Rate1600 cc/m²/day 23°C/0% RH; DIN 53380
Melt Flow3.45 g/10 min 190°C/2.16 kg; ISO 1133

Mechanical Properties
Elongation at BreakMin 50 % 50 mm/min; Nominal; ISO 527

Thermal Properties
Melting Point112 °C 10 K/min

Optical Properties
Transmission, Visible82 % ASTM D1003

Descriptive Properties
ColorTransparent 
Commercial Status (March 2007)North America and Europe 
Impact ModifiedNo 
Primary Processing TechniqueBlown Film 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.