Arkema Group RILSAN® Fine Powders Polyamide 11


Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic

Material Notes:
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum products.
Typical Applications:

  • Shopping carts
  • Dishwasher baskets
  • Hand mixers
  • File rods
  • Wire shelves

Information provided by Arkema Group

Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate38 - 47 MPa 
Taber Abrasion, mg/1000 Cycles17 CS 17 wheel, 1 kg load

Electrical Properties
Volume Resistivity3.5e+014 ohm-cm 20°C and 65% RH at 500 V; ASTM D257
Surface Resistance2.4e+014 ohm 20°C and 65% RH at 500 V; ASTM D257
Dielectric Constant3.1 1 MHz
Dielectric Constant, Low Frequency3.9 100 Hz
Dielectric Strength30.5 kV/mm 0.4 mm thick

Thermal Properties
Heat of Fusion83.7 J/g 
CTE, linear 20°C150 µm/m-°C 

Descriptive Properties
Flammabilityself-extinguishing ASTM D 635 (measured at a thickness greater than 3mm to eliminate the influence of substrate)

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.