Material Notes:
Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDER

Unpigmented and clear Powder as an additive for paints. Improves the scratch and abrasion resistance of paints. Allows for different texture depending on the granulometry used. Can be dispersed completely in liquid media.

Excellent chemical resistance.

The range includes several colors.

The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.04 g/cc0.0376 lb/in³ 
Water Absorption1.9 %1.9 % 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm1e+014 ohm-cm 
Surface Resistance1e+014 ohm1e+014 ohm 
Dielectric Strength30 kV/mm762 kV/in 

Thermal Properties
Melting Point185 °C365 °F 10°C/min
Vicat Softening Point160 °C320 °F 50°C/hr; 50N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94V-2V-2 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.