MatWeb, The Online Materials DatabaseArkema Rilsan® Powder ESY Black X 7260 Nylon 11, Coating GradeSubcategory: Nylon; Nylon 11; Polymer; Thermoplastic Close Analogs: Key Words: PA11; Polyamide 11 Material Notes: Melt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven. There is a wide range of colors. The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule. ISO data provided by the manufacturer, Arkema.
|
|||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Copyright 1996-2010 by Automation Creations, Inc. The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb. |