MatWeb, The Online Materials Database

Arkema Rilsan® Powder ESY Black X 7260 Nylon 11, Coating Grade


Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA11; Polyamide 11

Material Notes:
Powder ESY BLACK X 7260 - RILSAN POLYAMIDE 11 (PA11) POWDER

Melt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven.

There is a wide range of colors.

The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.35 g/cc 
Water Absorption1.9 % 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm 
Surface Resistance1e+014 ohm 
Dielectric Strength30 kV/mm 

Thermal Properties
Melting Point185 °C 10°C/min
Vicat Softening Point160 °C 50°C/hr; 50N
Flammability, UL94HB 1.6 mm
Flammability, UL94V-2 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.