MatWeb, The Online Materials Database

Arkema Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,EHLS,22-010,CD10

Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.

Very low friction coefficient. No need of lubricant. Excellent wear and chemical resistance. Long service life.

Example applications: Control cables tubing, parking brake control cable, cable for opening doors.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.07 g/cc 
Water Absorption1.4 % 
Melt Flow2.1 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield50 MPa 50 mm/min
Elongation at Break33 % Nominal Strain; 50 mm/min
Elongation at Yield5 % 50 mm/min
Tensile Modulus2.36 GPa 1 mm/min

Electrical Properties
Dielectric Strength34.1 kV/mm 
Dissipation Factor0.000358 1 MHz
Dissipation Factor, Low Frequency0.000411 100 Hz
Comparative Tracking Index600 V 

Thermal Properties
Melting Point174 °C 10°C/min
Flammability, UL94V-2 3.2 mm
Flammability, UL94V-2 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.