MatWeb, The Online Materials Database

Arkema Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,EHLS,22-010,CD10

Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.

Very low friction coefficient. No need of lubricant. Excellent wear and chemical resistance. Long service life.

Example applications: Control cables tubing, parking brake control cable, cable for opening doors.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.07 g/cc 
Melt Flow2.1 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield45 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield7 % 50 mm/min
Tensile Modulus2.2 GPa 1 mm/min
Charpy Impact Unnotched13.3 J/cm² 
Charpy Impact, Notched, Low Temp0.42 J/cm² at -30°C
Charpy Impact, Unnotched Low Temp11.1 J/cm² at -30°C
Charpy Impact, Notched0.45 J/cm² 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm 
Surface Resistance1e+014 ohm 

Thermal Properties
CTE, linear 20°C80 µm/m-°C Parallel to flow
Melting Point174 °C (Dry)
Deflection Temperature at 0.46 MPa (66 psi)162 °C 
Deflection Temperature at 1.8 MPa (264 psi)65 °C 
Flammability, UL94V-2 3.2 mm
Flammability, UL94V-2 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.