Material Notes:
Designation ISO 1874-PA12-P,EHL,22-004

Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.

High impact strength. High burst pressure. Very good chemical resistance. Easy to be processed.

Example applications: Pneumatic control tubes, Fuel line.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.04 g/cc0.0376 lb/in³ 
Water Absorption1.2 %1.2 % 
Melt Flow5.6 g/10 min5.6 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield26 MPa3770 psi 50 mm/min
Elongation at BreakMin 50 %Min 50 % Nominal Strain; 50 mm/min
Elongation at Yield24 %24 % 50 mm/min
Tensile Modulus0.465 GPa67.4 ksi 1 mm/min

Thermal Properties
Melting Point168 °C334 °F 10°C/min
Flammability, UL94HBHB 3.2 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.