Arkema Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12-P,EHL,22-004 Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized. High impact strength. High burst pressure. Very good chemical resistance. Easy to be processed. Example applications: Pneumatic control tubes, Fuel line. ISO data provided by the manufacturer, Arkema.
Physical Properties | Metric | English | Comments |
|
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Melt Flow | 5.6 g/10 min | 5.6 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 24 MPa | 3480 psi | 50 mm/min |
Elongation at Break | Min 50 % | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 25 % | 25 % | 50 mm/min |
Tensile Modulus | 0.415 GPa | 60.2 ksi | 1 mm/min |
Charpy Impact Unnotched | NB | NB | |
Charpy Impact, Notched, Low Temp | 0.39 J/cm² | 1.86 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | NB | |
Charpy Impact, Notched | NB | NB | |
Electrical Properties |
|
Electrical Resistivity | 1e+011 ohm-cm | 1e+011 ohm-cm | |
Surface Resistance | 5e+011 ohm | 5e+011 ohm | |
Dielectric Strength | 24 kV/mm | 610 kV/in | |
Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 140 µm/m-°C | 77.8 µin/in-°F | Parallel to flow |
Melting Point | 168 °C | 334 °F | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 125 °C | 257 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 46 °C | 115 °F | |
Vicat Softening Point | 130 °C | 266 °F | 50°C/hr; 50N |
Flammability, UL94 | HB | HB | 3.2 mm |
Flammability, UL94 | HB | HB | 1.6 mm |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|