Material Notes:
Designation ISO 1874-PA12-P,EHL,22-004

Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.

High impact strength. High burst pressure. Very good chemical resistance. Easy to be processed.

Example applications: Pneumatic control tubes, Fuel line.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.04 g/cc 
Melt Flow5.6 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield24 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield25 % 50 mm/min
Tensile Modulus0.415 GPa 1 mm/min
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.39 J/cm² at -30°C
Charpy Impact, Unnotched Low TempNB 
Charpy Impact, NotchedNB 

Electrical Properties
Electrical Resistivity1e+011 ohm-cm 
Surface Resistance5e+011 ohm 
Dielectric Strength24 kV/mm 
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C140 µm/m-°C Parallel to flow
Melting Point168 °C (Dry)
Deflection Temperature at 0.46 MPa (66 psi)125 °C 
Deflection Temperature at 1.8 MPa (264 psi)46 °C 
Vicat Softening Point130 °C 50°C/hr; 50N
Flammability, UL94HB 3.2 mm
Flammability, UL94HB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.