Arkema RilsanŽ AESN Y T6L Nylon 12, MoS2 Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,EHLS,22-010,MD05

Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.

Low friction coefficient. No need of lubricant. Good impact strength. Easy to be processed.

Example applications: Control cables tubing, parking brake control cable, cable for opening doors.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.04 g/cc 
Water Absorption1.6 % 
Melt Flow1.6 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield50 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield5 % 50 mm/min
Tensile Modulus1.8 GPa 1 mm/min
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.49 J/cm˛ at -30°C
Charpy Impact, Unnotched Low TempNB 
Charpy Impact, Notched0.48 J/cm˛ 

Thermal Properties
Melting Point174 °C 10°C/min
Flammability, UL94V-2 3.2 mm
Flammability, UL94V-2 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.